图片2

Cement Mortar Waterproof

It is a kind of flexible, rigid two-component polymer modified cement based waterproof coating.
Components:

(1) organic emulsion (made from high-grade acrylate emulsion and various additives)

(2)  and nonorganic powder (composed by special cement and multiple fillers)

based on a certain proportion.

Features:

(1) Non-toxic, pollution-free water paint
(2) Can be directly applied to concrete surface
(3) Cold construction, no restriction on substrate water content, easy in operation and short in construction time
(4) Superior adhesive performance

图片1

 

 

 

图片2

Application:
(1) Applicable to cellar, toilet, kitchen, floor, balcony, water pool etc. for waterproofing
(2) Typical Cases: the Great Hall of the People, the Three Gorges Dam, the National Swimming Center (Water Cube), etc.

 

图片1

waterproof cement composite board

The XPS Tile backer board is made of foam board in the core and coated with fiberglass and cement polymer motar on both sides. The range of flat panel in thickness is from 6mm to 80mm The tile backer board can be for floors and walls. It can be fixed directly to timber or cement floors and walls. When used as a structural tile backer board in the floor. It will save you money when used in conjunction with under tile heating by acting as a very efficient thermal barrier; it reflects the heat upwards into the floor tile instead of allowing heat to warm up the concrete slab below.

Characteristics: 

1 Low weight,10pcs of 10mm board is only 12KG
2 High compressive strength(about 350Kpa)
3 Waterproof, excellent for wet room.
4 Excellent for heat and sound insulation
5 Easy to be but with knife and saw
6 It’s CFC free, environment friendly board.

图片1  图片2

图片3  图片4

图片5  图片6

图片1

Expose how BAD quality insulation system Make?

This is a prefix in the development of housing prices in Shenyang high-rise building, a large area off the wall appeared in the

Western Hills area. Of course, a problem occurs insulation system, to scientifically analyze the reasons for its formation, the

conclusion that can not be easily materials, construction, or any other reason, but on-spot survey, scientific analysis of the

causes.

We look at this building has cracks in exterior latex “aspect terraced rice paddies” of the crack from the outside and inside.

Photographed in the top

图片2

The protective layer and the gap has been facing layer tear

图片3

Protective layers and layers of plaster finishes have more than 150 square meters off

A closer look at shedding interface

图片4

 

Remote observation off the wall

图片5

Falling plaster on the inside was pink, the residual thermal insulation material, visible on the fracture surface of the insulation

material, touching the exposed insulation layer, the feeling has been pulverized.

Sticking plaster above the fracture surface insulation materials

图片6

At the top level, we have a close look at some of the sheet crack, warpage.

图片7

Since the insulation board and the protective surface layer are cracks, then what is the key cause lead to the result? A

protective surface cracking, water, leading to cracking of the insulation board, insulation board or cracking resulting protective

surface cracking, or no relationship between the two? From the graph it seems that we can conclude is that tension plate

cracking, resulting protective surface cracking.

We found mortar bonded insulation board and the place has become a dark color, touch found the site has been chalking

discoloration, loss of mechanical strength. But not discolored parts still have a certain hardness.

p03-04

PU Thermal-insulation boards

Installation Method

(一) Layering Type
A delicate and highly elongated adornment line, give a person a higher longer visual sense, lively line concise artistic conception.
Features:
1. The prefabricated installation, do homework, modular, convenient and quick.
2. The solid structure, removable, can repair.

打印

(二)The Back Hanging
Appearance is concise, lively.
Features:
1. The structure is stable, safe
2. Easy installation and adjustment
2. The reserved crack-cleaning constructive ventilating curtain wall system

p13-14

(三) The Visible Order Type
Safe and reliable, convenient and quick installation, the economy is good, adornment nail and plate color match reveal the beauty of the rugged

p13-14

(四) Embellishment (plus anchor)
Easy installation, economy, takes up less space
Fastening methods: st

p03-04

Modified EPS Thermal-insulation Boards

Installation Method

(一) Layering Type
A delicate and highly elongated adornment line, give a person a higher longer visual sense, lively line concise artistic conception.
Features:
1. The prefabricated installation, do homework, modular, convenient and quick.
2. The solid structure, removable, can repair.

打印

(二)The Back Hanging
Appearance is concise, lively.
Features:
1. The structure is stable, safe
2. Easy installation and adjustment
2. The reserved crack-cleaning constructive ventilating curtain wall system

p03-04

Reinforced Fibrous Composite Thermal-insulation Boards

Installation Method

(一) Layering Type
A delicate and highly elongated adornment line, give a person a higher longer visual sense, lively line concise artistic conception.
Features:
1. The prefabricated installation, do homework, modular, convenient and quick.
2. The solid structure, removable, can repair.

打印

(二)The Back Hanging
Appearance is concise, lively.
Features:
1. The structure is stable, safe
2. Easy installation and adjustment
2. The reserved crack-cleaning constructive ventilating curtain wall system

p13-14

(三) The Visible Order Type
Safe and reliable, convenient and quick installation, the economy is good, adornment nail and plate color match reveal the beauty of the rugged

p13-14

(四) Embellishment (plus anchor)
Easy installation, economy, takes up less space
Fastening methods: structural adhesive, double-sided adhesive sticky tape

p13-14

(五)Card Type (insulation system)

p13-14

(6) Closed

p13-14

Technical parameter:

Testing terms Testing reference Testing conclusion
Thickness(mm) GB/T 17748-1999 4-12mm
Dimension(mm)
Dimension Deviation Length(mm) ≤2 -1
Thickness(mm) ≤0.05 -0.5
Diagonal difference(mm) ≤2 2
Fringe nonstraightness(mm/m) ≤2 1
Warpage(mm) ≤5 2
Density(g/cm3) ≥1.6 1.6-1.7
Resistance to change of temperature GB/T 17748-1999 Had no effect on
Dry shrinkage rate JC/T671-1997 0.07
Water absorption(%) ≤5 1.79
Water impermeability GB/T019-1999 Without dripping in the bottom
Coefficient of thermal expansion GB/T17748-1999 8*10-6
Thermal conductivity ≤0.5W/mk 0.3W/mk
Elastic modulus ≥8000N/mm2 9000N/mm2
Drawing bolt force(N/mm) Normal JC/T564-1994 190
Warm 234.9
Incombustibility GB545640-1985 A级
Flexural strength(Mpa) GB/T7019-1997 38.8
Resistance to shock strength(KJ/m2) GB/T25741-1995 4.74
Frost resistance Without dusting or peering off after 15times of freezing-melting circulation Without failure phenomena of dusting or pearing off
Color  Solid/meta;/pearlized color
60℃ Iuster GB/T9754-1988 Low/mid/high glazing
Hardness GB/T6739-1996 2H-4H
Resistance to change if temperature GB/T17748-1999 -40-150℃,Unchanged
Resistance to solvent GB/T17748-1999 Butanone>not expose the basicboard when soaking in butanone 100times
Acid resistant GB/Y17748-1999 Had no effect on
10%HCL24h
10% sulfuric acid 24h
Alkali resistant GB/T17748-1999 10%NaOH 24h Had no effect on
Resistance to detergent 3% 40℃ Had no effect on
Weather resistance GB/T16259-1996 Luster loss than 30% within 3000 hours, color changes not over than 5NBS
Insolation outdoors ASTM D-2244-85 Luster loss than 50% on outside of 10 years, color changes not over than 5NBS
p03-04

Mineral Wool Thermal Insulation Boards

Installation Method

(一) Layering Type
A delicate and highly elongated adornment line, give a person a higher longer visual sense, lively line concise artistic conception.
Features:
1. The prefabricated installation, do homework, modular, convenient and quick.
2. The solid structure, removable, can repair.

打印

(二)The Back Hanging
Appearance is concise, lively.
Features:
1. The structure is stable, safe
2. Easy installation and adjustment
2. The reserved crack-cleaning constructive ventilating curtain wall system

p13-14

(三) The Visible Order Type
Safe and reliable, convenient and quick installation, the economy is good, adornment nail and plate color match reveal the beauty of the rugged

p13-14

(四) Embellishment (plus anchor)
Easy installation, economy, takes up less space
Fastening methods: structural adhesive, double-sided adhesive sticky tape

p13-14

(五)Card Type (insulation system)

p13-14

(6) Closed

p13-14

Technical parameter:

Testing terms Testing reference Testing conclusion
Thickness(mm) GB/T 17748-1999 4-12mm
Dimension(mm)
Dimension Deviation Length(mm) ≤2 -1
Thickness(mm) ≤0.05 -0.5
Diagonal difference(mm) ≤2 2
Fringe nonstraightness(mm/m) ≤2 1
Warpage(mm) ≤5 2
Density(g/cm3) ≥1.6 1.6-1.7
Resistance to change of temperature GB/T 17748-1999 Had no effect on
Dry shrinkage rate JC/T671-1997 0.07
Water absorption(%) ≤5 1.79
Water impermeability GB/T019-1999 Without dripping in the bottom
Coefficient of thermal expansion GB/T17748-1999 8*10-6
Thermal conductivity ≤0.5W/mk 0.3W/mk
Elastic modulus ≥8000N/mm2 9000N/mm2
Drawing bolt force(N/mm) Normal JC/T564-1994 190
Warm 234.9
Incombustibility GB545640-1985 A级
Flexural strength(Mpa) GB/T7019-1997 38.8
Resistance to shock strength(KJ/m2) GB/T25741-1995 4.74
Frost resistance Without dusting or peering off after 15times of freezing-melting circulation Without failure phenomena of dusting or pearing off
Color  Solid/meta;/pearlized color
60℃ Iuster GB/T9754-1988 Low/mid/high glazing
Hardness GB/T6739-1996 2H-4H
Resistance to change if temperature GB/T17748-1999 -40-150℃,Unchanged
Resistance to solvent GB/T17748-1999 Butanone>not expose the basicboard when soaking in butanone 100times
Acid resistant GB/Y17748-1999 Had no effect on
10%HCL24h
10% sulfuric acid 24h
Alkali resistant GB/T17748-1999 10%NaOH 24h Had no effect on
Resistance to detergent 3% 40℃ Had no effect on
Weather resistance GB/T16259-1996 Luster loss than 30% within 3000 hours, color changes not over than 5NBS
Insolation outdoors ASTM D-2244-85 Luster loss than 50% on outside of 10 years, color changes not over than 5NBS